Letter 2036

--

We have palladium-nickel alloy plated rejects which we wish to strip the plated palladium-nickel and reclaim the palladium with chemical precipitation. Plaese advise,thank you

Keat-Seng Ong AMPMAS SDN.BHD. - Penang, Malaysia


--

Contact Thom Anderson, WIT Sales & Refining, San Jose, CA, USA, for suggestions.

Mandar Sunthankar