How to electropolish Nitinol for microstructure studies

--

I am interested about the electropolishing, chemical polishing of Nitinol for Microstructure studies using optical microscope and scanning electron microscope.

Ganesh Kumara K.
Mangalore University - Mangalore , Karnataka


.

hi ganesh

i have been trying my own luck at EP Nitinol for optical and electron microscope studies. The idea here is to get a good surface finish which can be done with a fine diamond polish.

for EP a good solution to use would be 20% H2SO4 in methanol. You can connect it as the anode to have faster removal of the oxide and then later try to polish it at the cathode with hydrogen evolution. But you need to do a couple of trials to get your own recipe as it depends on the distance of the electrodes, surface area, current density etc.. I would suggest using low to medium voltages (around 10 V) to get a steady uniform removal. In the meantime if u have had any luck with this please do let me know as I will be interested with your progress. I have a few relevant pubs. if u are interested.

-- Guru

Guruprasad Ramanathan
Case Western Reserve Univ. - Cleveland, Ohio


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search