Could someone please provide me with a breakdown of materials in Inconel? (Including percentages of each).I am told that it contains: nickel,chrome,columbium and titanium. Is this correct and are there any other constituents? Any help would be greatly appreciated.

Jeff Mills
metal finishing shop - Gorham, Maine


--

Inconel is 14 percent Cr, 6 percent Fe, balance Ni. See the Electroplating Engineering Handbook for more info


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


-

I seem to remember , at college, being told that the name "Inconel" was actual made up from some abbreviations, possibly of metals. Does anybody know where the name "Inconel" actually came from ? Thanks, Colin.

colin parsons
- Saudi Arabia


++

INCONEL--THIS IS A TRADE NAME OF INTERNATIONAL NICKEL. I HAVE MOST OF THEIR LITERATURE AND WILL ANSWER ANY QUESTIONS TO DO WITH NICKEL ALLOYS AND STAINLESS STEEL.

ROBERT RIDDOCH
- MONTREAL, QC, CANADA


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com