Platinum embrittlement
--
is hydrogen brittlement [a problem with] platinium metals at hight temperature.(960°C)?
Paquin Ludovic
--
Pt-metals, Au and Ag deposited from aqueous or organic solutions contain H2 which is essentially removed at 400-600 C. Warning: powders may explode in air.
Alex Kozlov
- New Jersey