CHEM FILM ANALYSIS TESTING
+++I AM INTERESTED IN SETTING UP IN HOUSE TESTING FOR OUR CHEM FILM PROCESS TO Mil-C-5541 [link is to spec at TechStreet]. WHAT DO I NEED AND IS THERE A MACHINE THAT WILL DO THE TESTING AUTOMATICALLY.
DAN KAISER- HICKSVILLE, New York
+++
Solution Analysis including Cleaning Solutions - Weekly
Salt Spray Testing per ASTM ASTM B-117 [link is to spec at TechStreet] - Monthly 5 panels 0.020 x 3 x 10" at 6 Degrees for 168 Hours
Adhesion (if applicable) - Monthly
Visual - Every Lot
Nothing here is automatic, and you need to look after/document the salt spray unit twice a day.