Aging Magnesium

+++

I have a pair of real magnesium automobile wheels, mfg. by American Racing from the 1950's. As you know magnesium turns black over time. I cleaned the wheels up as they were very stained. What I would like to know, is, how to speed up the aging process that turns the wheels black? I am looking for an even black color.

Thank You,

Paul Hattrup
- Irvine, California, USA

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search