How to obtain deeper well aligned porous titanium dioxide?

 

+++

I have obtained well aligned porous titanium dioxide by using anodizing technique, but only about 300 nm depth, how to get deeper ones, for about several micrometers?

Qunliang Song
- Shanghai, P.R.China

Ed. note: please explain whether you used alkaline or acid anodizing, and what electrolyte and voltage you used. Thanks! Anodizing is a self-limiting process because the anodized film is a resistor that stops permitting passage of current at a given voltage after a certain thickness has been obtained.


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search