Converting Rz measurements to Rms measurements
+++
I'm looking for information for converting surface finish specifications measured in "Rz" to those measured in "Rms". This would be mainly on steel parts. Thanks for the help.
Kay Kucharik
- Solon, Ohio
|
+++
Rz is the same as RMS; however, the Rz spec designates a specific number of ridges and valleys (5) to be traversed by a profilometer.
|
AF Kenton
Huntingdon Valley, Pennsylvania
|
| |