Nickel acetate solution?

+++

Need a formula for a nickel acetate solution for my anodizing line. It's small scale. Any helpful hints on this type of sealing process greatly appreciated.

Michael Baunach
- Louisville, KY, USA


+++

Nickel Acetate conc: 0.5-1.0 oz/Gal temp: 195-205 deg F preferably DI water

Dado Macapagal
- Toronto, Ontario


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search