Dear sir,

I would like to ask u question about zinc phosphate pre-treatment. I'm facing some problem of sludge which is by product of the phosphate reaction its in form of ferric phosphate. Too much sludge generation and the nature of sludge is sticky so its damaged my wires surface when its drawing. Will u suggest an additive to less the sludge or to help out to convert that sticky nature in smooth one so I can easily wash it out with water. Waiting for ur help.

Willium Dias
- Bombay, India


First of two simultaneous responses -- +++

Hi Willium,

It is difficult to answer your question because the answer lies in the process details. Sludge formation can be controlled by altering the ration free to total acid. It is also dependent on accelerator concentration.

Check your bath parameters to ensure that they are within specification. This is the #1 cause of problems in phosphating baths because operators do not pay close enough attention to these important details. Then ask your pretreatment supplier to recommend conditions that will minimize sludge formation.

George Gorecki
- Naperville, Illinois


Second of two simultaneous responses -- +++

You can use calcium zinc phosphate solution. This will reduce sludge formation.

Harish Chitkara
- Chennai, Tamil Nadu, India


+++

DEAR WILLIUM,

You can remove sludge by installing a clarifier which can pump out the sludge and give clear and green soln of phosphaste which can be reused. This will also save your money.

Thanks,

NAIR VIJAYAN R
- MUMBAI, MAHARASHTRA, INDIA


+++++

Dear William,

It always happens when a loss in chemical eqb is happening in your baths. Check for carry over of one bat to other. We faced a similar problem which was later corrected when we prevented carry over from Activation to Phosphating and Phosphating to Rinse.

I am sure these precautions might help you as well...!

Regards,

Mohit J Saraf
shock absorber mfgr. - Indore, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search