HOME
FAQs
BOOKS
JOBS: Help Wanted
Suggestions
you are here: Hotline/Forum =>
Letter 19054
Satin chrome plating
+++
I wanted to know how to specify on a drawing to have an aluminum part made from adc 12 (a die-cast alloy equivalent to a380) to be first electroless nickel plated (class 3) then have a very thin layer
(splash/flash?) of satin chrome plated on top of that.
Greg Arcenio
- Palo Alto, California, USA