Dichromate seal for anodizing aluminium

+++

HI!

WE ALREADY HAVE A SMALL SET-UP FOR ANODIZING AND WE LIKE TO DO DICHROMATE SEAL ON PARTS (LOOKS LIKE GREEN-YELLOW).

WHERE DO I CAN FIND INFORMATION ABOUT THIS PROCESS?

THANK YOU,

STEVE POUDRIER
- Victiriaville, Quebec, Canada


+++

The book The Surface Treatment and Finishing of Aluminum and Its Alloys by S. Wernick, R. Pinner, P.G. Sheasby has the info you need.

Dado Macapagal
- Toronto


+++

We used to prepare dichomate seal: Concentration: Sodium Dichromate 7 oz/Gal Temp.: 195-205 deg F DI water

Dado Macapagal
- Toronto


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search