++++ I am trying to find the easy way for separating copper from 14 kt. scrap? anything faster than sodium nitrate glass etc. and than cupeling this and breaking off the glass ect. ect. Craig Griffin
++++ I have a fairly large amount of gold in solution. I've evaporated off the nitric and now it's in hydrochloric acid. Can anyone tell me what will precipitate the gold? Also, will nitric remaining in the solution influence the precipitation and if so, how can I test for it. Tim Roberts
++++ I have about 100 lbs. of low-grade gold plated eyeglass frames. My goal is to recover the gold myself. I have done some experimenting and it appears that melting them and constructing some type of Mobius or Thum cell would be the best approach. I am open to suggestions on all parts of this project Mike Rotalsky
++++ I am involve in a research project to recover gold from electronic scrap. The sample that I am working with have a high concentration of copper compared to gold. Hence, this makes the recovery process of gold difficult. Is there any method or sorbents that can separate gold from copper? The concentration of the copper is about 10 times more than gold in my sample. Ryan Tong
++++ I WOULD LIKE TO KNOW MORE OR LESS HOW MUCH GOLD ONE CAN REFINE OUT OF A 1000 POUNDS OF COMPUTER MOTHERBOARDS.(RANGING FROM 486 TO P1)? Dirk Walters
++++ Tim, When you have the solution in HCL form and works if it has some HNO3 left in it (perhaps better) you can dilute it with water, about 2000 Ml. and after bringing to a boil add "Potato White" which is sodium metabisulfite while stirring (use three times as much "PW" as gold as you anticipate) (You can buy it at a chemical supply house as a food grade very cheaply) . Then add more "PW" and see if you get a cloud, if you do you are precipitating more gold. Try a small amount and be sure there is a small Amount of HNO3 still in the solution and that it is dilute enough to be able to see through it with a light behind it. If there is no more clouding let it cool and settle then filter through a tight filter. If you have any white precipitate you have added too much "PW" not that it will hurt but give you an indication for the next trial. The good stuff will look like coffee grounds sort of. Place the solids in a new beaker and boil with water to clean the white material out. or I would just melt the entire batch in a crucible and you will have pretty good gold. about 95% or better. I add pure lead and 4 parts silver then use a cupel to separate the gold from anything else and get about 99% Good luck Adrian Meador
++++ Tim, In the last note I neglected to add that you need to part the cupelled button with 50% nitric acid to dissolve the silver and leave the gold in a very pure state. Adrian Adrian Meador
++++ I have about 10 lbs of scrap electronic pins and fingers and would also like to refine scrap jewelry. Would it be worth my while to spend $600.00 on refining equipment to under take this task? The equipment I am referring to is the simplicity sold by Shor. Carl Nagl
++++ I have a few pounds of gold plated electrical components. Most are very small pieces. I just read that you should never use AR for platings. My question is, How do I recover the gold? Every refinery that I've asked is not interested in plated gold. Who should I contact? Gregg Bremers
++++ I am interested in removing the gold from circuit boards and was wondering if you could remove it strictly by using electricity. Thank you, Dan Pridgen
++++ As simple as I can state it. One computer contains approx. $1.20 in precious metals and it cost approx. .80 cents to retrieve it (and that is, if you do the recovery perfectly), so you profit .34 to .40 cents . Notice I said one computer... you can strip it down to the boards, chips, and pins and still going to profit 34 to 40 cents each. hope this helped. Frankie Burk
++++ this inquiry added to an existing thread by the editors Need to know how to remove gold from circuit boards.step by step in laymen's terms. I'm not super smart so please explain in steps. I would appreciate any advice. I have access to lots of old computers and would like to recycle as much as possible. Thanks, John minn
+++++ The gold in the west electronics is very rare about 4 g/kg. But in the former Soviet Union and satellites the situation is different. Today I got 15 g 22 karat gold from a single computer, made before 22 years in Bulgaria, this is a gold mine. I understand that the old machines in the east Europe and Russia are gold mine!!! Ivan Georgiev
+++++ Hi, I'm a business man engage in buying any kind of scrap such as an electronic scrap. With this, I have collected plenty of IC's (integrated circuit) from these electronic scrap. I have at least 30 kilos of LQFP and QFP package of IC's with different number of pins from 44 pins to 144 pins. I would like to know how much ounce of gold I can get from these IC's. I would like to recover the gold from these IC. With this, I have performed an experiment using sulfuric acid to melt the molding compound of the IC's and then sort gold wires from the melted molding compound and copper pins. This is a long and expensive process so I stop the experiment. Instead, I use the aqua regia to recover the gold. By heating the IC's with aqua regia at 300 C the IC's (molding compound, copper pins and gold wire) were dissolved leaving the molding compound at the bottom. Then I filtered the solution and neutralize the nitric acid using a urea. After doing all this I'm not successful in precipitating the the gold, using sodium sulfite. What I get was a black powder and white powder at the bottom. I burn to melt these powders and obtain a black colored metal not gold. If somebody from you guys out their who have experience in recovering the gold from IC's can you please share to me some tips or more accurate, economical and safer process that what I'm doing. I already tried three times in perfecting the aqua regia process to recover the gold from my IC by not Successful. Desperate to for your help. Alex Master
+++++ I have used aquaregia to dissolve gold and silver from e-junk. Can the electroplating system be used to bring the dissolved gold back to gold metal? If it can be done what material should the anode and cathode be ? What acid should be used? Also, how and what is used to bring back the dissolved silver? BILL Luxmore
+++++ directed mostly to Richard Alcorn Richard you mentioned making AR in situ with sodium nitrate and HCl. Can you elaborate on this a little more. Thanks Jim Wiggins
+++++ It seems like we all have something in common. Those who have the answers won't share them. I have had some success in extracting the gold off of connectors and "broken fingers" using "pcb etchant solution"from radio shack cat#276-1535. It takes longer than nitric,but is a lot safer. It works best when hot, not boiling, straight from the bottle. When dissolved, by using electrolysis on the copper the gold is easier to get too. Do not use this on aluminum. on the ceramic ic.s use hydrofluoric acid also know as glass etchant to dissolve the casing. but,when all ELSE FAILS I use Abington Metals in Philadelphia, PA USA as my refinery. Linda Thier is a great help,if you don't know what you have, send her a sample and she will tell you what it is and if is worth anything I hope this helps someone. Doug Russell Ed. note: I don't think it's fair to characterize the readers with "those who have the answers won't share them". Just on this one thread alone some exceptionally informative postings have been offered by Panjala Mukesh, Richard Alcorn, Peter Couture, Adrian Meador, and others.
+++++ Gold containing article is made anodic and is stripped electrolytically , or is immersed in the above mentioned solution of NaCN, NaOH, and SMNBS.
+++++ We just acquired a very large surplus of computers & need to know what parts have gold on them. We don't know what "chips",connectors etc., we don't know one chip from another. Is there a diagram that shows what parts are salvageable? How do you refine it? Debbie Smith
+++++ Have removed most of gold and other metals from 32 yrs old
computer now what do I do with it help me please my husband was Vol.
Fireman who was disabled in line of duty this is something he started
before totally disabled and we could use any financial help possible
he was sure when he did it was good thing been sitting here about 7
yrs. If you have suggestions please. Kathy L Doench
+++++ While there may have been more gold on typical electronics in 1973 than today, computers use a few millionths of an inch thickness of gold, the parts are not made of solid gold. I hate to have to be the one to tell you, but the value of the gold from a 1973 computer probably won't buy more than a Happy Meal. But take it to any jeweler or pawn shop who says they buy gold, and see what they say.
+++++ My experience is to take a fresh razor blade and follow the printing of the board and remove as much as you can. This is very time consuming but it will save you money on acids due to scraping the gold into a smaller quantity. I personally would not do it if there were hundreds of boards but for a few and experimenting it saves space and money. If not sell on EBAY. Holly Figueroa
+++++ For those that are trying to refine electronics, maybe this will
help you. I use this process for refining all gold including
electronics. Maurice Robinette ----
I like everyone else it seems have several hundred pounds of motherboards, ethernet, etc scrap as well as telephone scrap that I need to process. What I have been doing is pulling the cpus and cutting fingers and selling via the internet. What I wonder is what is remaining on the boards and how do I remove it. I think the jumper pins, ide connector, pci slots, etc are gold plated but after many attempts at many methods I have yet to find a way to efficiently remove the pins from the boards. The worst seems to be the pci type slots that just won't let the pins come out of the assembly. Is there a product, acid mixture, or solvent that will dissolve the plastic material and leave only the metal pins? I remove the pin assemblies with a small Dremel tool just clipping the bottom of the leads but the plastic is a very big problem so far. Any help is very greatly appreciated!!! Thanks!!! Chris Coleman
January 25, 2006 Lots of people seem to be interested in doing this. I found a guy
on eBay selling old chips and he said "gold recovery" and I did a
little google search and ended up here. Zi Mei
January 30, 2006 Hello, Johnny K
January 29, 2006 To all the "Experts", william bemis
January 30, 2006 Please share your expertise and write down the steps for us to go save someone who is in a burning building, William :-) Would you not urge people to call 911 instead? And if they have an abiding interest in the subject, then urge them to get hands-on training and qualification testing in lifesaving, read books on the subject, and don't attempt it unless they have the right equipment? That's exactly what I and many readers have done on this thread a dozen times and counting. An internet posting is a "one room schoolhouse" with ten thousand people wandering in and out; some are 3rd graders and some are PhDs, some have decades of safety training and some haven't a clue, some are working in well established research labs and some are trying to work on their kitchen stove, some are your neighbors and some are desperate third-worlders clutching at any scheme to feed their starving children, not next week but today. If they know enough about the subject to frame a specific question, I think the experts will answer it, but I think "full answers" that can make things safe for all readers is a total impossibility, and that all we can do is to continue to tell people not to work with hazardous chemicals without hands-on training in the subject and working in a proper industrial facility with the correct gear and PPE.
January 30, 2006 I think all these people inquiring about refining gold and silver from computer parts are all wasting their time. I agree with the general consensus that there is no significant amount of gold to be recovered from these sources. The health risks greatly outweigh the potential profit margin, if any at all. It amazes me to see people willing to risk their health, as well as the health of others in their immediate environments to get a tiny scrap of gold. Expending so much time and energy for the smallest returns. You could make far more money per week working at Mcdonalds and eat all the fattening food they sell for free. At least it would be a regular paycheck and even healthier for you too, if you can believe that. God help the get rich quick mind. Get a job, it pays more. Lol. Ryan Maximus
January 31, 2006 Don't make the mistake of thinking that I condone an untrained
person doing anything that is dangerous. William Bemis
January 31, 2006 And I will return again to an analogy to your line of work,
William. People will go into a burning building to save their pets
even though you tell them not to. So let me quote you -- Your first posting was right: people who are using these dangerous materials without hands-on training are "a danger to anyone within a hundred yards of them". People lacking a background in a subject and who will not get training at least should start by reading a book on that subject rather than expecting a one-paragraph internet answer. Otherwise, do we start by discussing fulminates? Or the dangers of perchloric acid? How to select goggles? Which respirator will be effective and which will prove useless for a given chemistry? How to dispose of the waste? The evolution of HCN gas from acidified cyanide? Heat of reaction? Treatment of chemical burns? Which safety topics do we omit?
February 2, 2006 Ted, First let me thank you for allowing me to have a voice here. Now then, This will be my final post. You guy's keep up the good work and keep me and all the other firefighter/medics in work. William Bemis
February 2, 2006 It would take far too long to acquire any decent amount of gold from electrical appliances, why not collect broken jewelry and when you have a sufficient amount for a small bar, melt it down using a crucible, these can be made or bought the electric crucibles work great although you can make one by using a oil drum cut down with a smaller drum in side and fill with concrete using fire proofing bore a small hole in lid attach a coupling to the wall and fit your gas supply using propane this is a hot burning clean gas, crucible goes inside with some borax powder and gold into the crucible and turn up the heat, about an hour later hey presto you got gold, advisable to melt the gold more than the melt heat for pouring, make sure you got a good bar mold preferably cast, you can make them out of clay or porcelain fired well, but these want last long,. Paul Bates
February 5, 2006 I too saw the Ebay sale for 10 lbs of "Recycling" CPUs and decided to research the topic. I am proud to say that I will NOT be attempting to conquer this chemistry experiment. I am smart enough to know NOT to try this. I'm sorry, but to spend $.80 to recover $1.20 in gold using toxic chemicals does not make sense to me. I can make more money cutting lawns! Steve Demers
February 12, 2006 I in no way plan to even try this, but find it interesting that people would consider such a dangerous task. Lack of understanding to the dangers I think. One question. Why wouldn't you grid to a fine powder, then separate by weight, then just melt out the gold? Gold is so heavy it should seperate easily and I don't understand the need for all the chemicals. The melting process would probably still leach some pretty toxic gasses, but less then all the acid use, as the other substances could be removed before melting. Anyway just my two cents worth. Oh yeah, working at McDonalds would provide a better income, I agree. Kevin Longbrake
February 12, 2006 I have experience in recovering gold from a variety of sources but
not specifically in e-scrap.I am posting this information on this
board to see if any one has attempted the recovery process on
e-scrap. Gopalan Ramadorai
April 20, 2006 If you have a lot of gold, you are in the gold refining
business. Alain Pelletier 1 2 3