Zn+Yellow passivation Technical details
++
Sir,
We are manufacturing deflection yoke and crossarm is one of the
component, Which will be plated(Zn plating thickness-5microns +
yellow passivation). To arrest our v-coil and crossarm,we used to
apply Polyamidesunmide resin(Temp-200'C) between v-coil and crossarm.
Here, we are facing decoloration problem in few of the components.
So, I am interested to know the passivation will withstand for
>150'C and if the answer yes. We required the chemical details and
specification.
Regards,
J.S.Rajan
- Bangalore, INDIA