Pickling Stains on Hot Rolled Steel

++

What are the long term effects of pickling stains on hot rolled steel? Are pickling stains corrosive? If a pickling stain is covered with a hybrid epoxy powder paint, will it start to peel off in several years?

Lennie D. Moore
Julius Blum, Inc. - Stanley, N.C., USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search