HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 18062
Stainless Steel Scratches
++
We put light scratches in a stainless steel sink and I was wondering what can take them out. I tried to look up "The Stuff for Stainless" and it wasn't clear on what to order..any other methods to take care of this or products I can use?
Necia R [last name deleted for privacy by Editor]Giummarra Electric - Crystal River, Florida
Ed. note: Finishing.com has a FAQ on this subject, and also a supporting advertiser, Scratch-B-Gone, who offer a new product designed for this purpose. Good luck, Necia.
+++++
Has anyone been successful for clearing scratches that are against the grain ?
I have a brand new stain less steel top on my sink tavle. when they were installing the sink vessel that goes on top, they really did a number on it. I wanted to cry!
Can any one help?
Thanks
Terry
hobbyist - Andover, Massachusetts