Stripped rims are oxidizing

++

I have a CBB929RR and I had stripped the paint of my rims and now they are oxidized BAD, what can I do? I have re sanded them and re sanded... I have re polished over and over. What are my options?

Thanks,

Rich Melillo
- Gretna, Louisiana


++

Lacquer! Polish them, then immiediately degrease and lacquer them, doesn't look much different from bare polished aluminium, except it doesn't corrode, I've used acrylic car lacquer with great success on copper and aluminium

George Ingram
- Swansea, Carms, Wales


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search