Letter 17518
What type of vinegar cleans a penny
better?
++
Hi! My name is Marvin. I'm doing a science fair project about
which knid of vineger cleans a penny the fastest. One of the
requirements is to interview an expert & since you are the expert
I'd like to interview you. Before I ask you a question, I would like
you to know that I would be using: white vineger, red wine vineger,
white wine vineger, rice vineger, & malt vineger (all added with
1 tsp of salt).
1. What is your name?
2. What is your field of expertise?
3. Have you done this experiment before?
4. Which vineger cleans a penny the best?
5. What chemical in this vineger cleaned the penny better?
6. Did the acidity of the vinegar made the difference?
Please respond ASAP as this is requirement for my experiment in
science. Thank you very much for your time and your technical
expertise. Andrsen Air Force BAse DODEA Guam Middle School.
Marvin
- Dededo, Guam, USA
++
Please tell your teacher that this "expert" feels that you have
been asked to do the project in the wrong order, Marvin.
You must first DO the experiment AND ONLY THEN compare your
results with what the "experts" have to say. To ask for the result
before you do the experiment will teach you to rely on hearsay
instead of experimental result, and to unconsciously jury-rig the
experiment to achieve the result you were told to expect. This is the
opposite of the "scientific method"; rather it is what we call "junk
science" -- a major plague today. It includes ignoring your own
results, altering the procedure, ignoring any wackiness of what
you've done, and just keeping at it until it gets you the results you
were looking for.
1) My name is Ted Mooney; 2) my field of expertise is metal
finishing; 3) I have done parts of the experiment before (I have
cleaned pennies with salt and vinegar several times) but I have never
compared different types of vinegar; 4) I don't know; 5) acetic acid
is the ingredient in vinegar that contributes the most to removing
tarnish from pennies; 6) the acidity is what does the job, so I would
expect the vinegar with the most acid to work the fastest.
My guess is that you will see no measurable difference in
performance between any of these vinegars. But that brings us back to
the beginning again, because I have now corrupted you into believing
the experiment will show no differences before you've even started
it. So as soon as you get some differences you will be tempted to
discount them and write them off as experimental error.
And we will have educated one more student into a lifetime of junk
science. So please do the experiment first! Keep a notebook with
numbered pages, write down everything in ink, never erase or yank out
any result. A proper lab notebook should get you an A on the project.
Good luck.
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|
Ed. note: For each metal finisher in the world
there are 10,000 students. The result is that we are drowning under
variations on this question alhough we've already answered similar
questions hundreds of times. Students please search the site for
those similar letters or read our F.A.Q. on the
subject ; sorry we cannot answer any more
questions on this.
 |