finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 17078

Sputtering vs. Vapor coating

++

When metallizing PET Film for Fabrication of solar control window film, Does sputtering have any advantages or superior charteristics versus vapor deposition when using Aluminum as metal?

Michael R. Byrd
- Hobe Sound, FL 33455


++

By vapor deposition I assume you mean ion vapor deposition, or IVD, a common means of depositing aluminum wherin the aluminum is evaporated. Sputter deposition of aluminum should result in a better coating -- the metal reaches the substrate with greater kinetic energy -- but is generally a much slower process, and therefore more expensive.

treglio portrait Jim Treglio
coatingservicesgroup

Lakeside, California

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search