Letter 16172 PURITY TEST FOR STAINLESS STEEL- 304 GRADE [India]++ HOW AM I SUPPOSE TO KNOW WHETHER A ROD GIVEN TO ME IS OF STAINLESS STEEL OF GRADE 304 i.e. HOW CAN I ASSURE MYSELF OF ITS PURITY SO THAT I AM NOT CHEATED BY THE FIRM FROM WHICH I SHALL BUY SS OF GRADE 304... SACHIN DEVENDRA CHACHADA
++ Either... (1) buy from a supplier that you trust, or whose certificate of chemical analysis you trust; or (2) have the material analysed by a commercial laboratory, so that you get an independent certificate of analysis. Bill Reynolds