Hi,

I have an Alnico (grade 5) alloy to etch. I don't have any references about that. Which reagent is commonly used and what will be the structure of my specimen. Do you have some pictures of it?

Thank you! Stéphane Godin
Hydro-Québec - Varennes, Québec, Canada


++

The most commonly used reagent for AlNiCo alloys is the Marbles's reagent. It'is made of 10g of CuSO4, 50 ml HCl and 50 ml of H2O. Immerse it for 5 to 60 seconds.

Stéphane Godin
HQ - Varennes, Québec, Canada


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search