HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum =>
ELECTRO POLISHING OF S.S. 420 GRADE
letter 16059 ++
DEAR SIR,
I WANT TO DO ELECTRO POLISHING ON STAINLESS STEEL 420 GRADE STRIPS PRODUCT KNOWN AS RIDERLESS HEALD'S USED IN TEXTILE WEAVING THE THICKNESS OF PRODUCT IS 0.30 MM, WIDTH IS 5.50 MM & LENGTH IS 280MM TO 410MM.
PLEASE GUIDE IN THE ABOVE MATTER.
MR. ASHOK M. NAIR-MAHARASHTRA, INDIA
++
Hello, Ashok. Most of the "must have" metal finishing books include good chapters on electropolishing of stainless steel, including the Metal Finishing Guidebook, ASM's Metals Handbook, Vol. 5., and especially the Electroplating Engineering Handbook, which has a great chapter on the subject.
Good luck.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |
++
Proprietary electropolishing processes for ss-400 series are available in India.
Ramesh Khare- Mumbai, India