Neutralizing agent

++

Sir,

We intend to manufacture Mild Steel Wires from wire rods and are interested to find out what neutralizing agent should be used after pickling the wire rod in Sulphuric Acid & rinsing with water.

Your answer will be highly appreciated.

Thanks,

Tarun Khandelwal
- Nashik, Maharastra, India


++

A silicated alkaline cleaner should be good.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++

It depends what you want to do with the wire after neutralising it. If it is not to be plated then the above remedy will offer you temporary corrosion protection only.

khozema Khozema Vahanwala
Saify Ind
 
Bangalore, Karnataka, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search