Rhodium plating

Ed. note; This is an interesting thread, but before you get too confused, you might want to start with our FAQ on Rhodium Plating and White Gold to get an overall understanding :-)

++

I just want to express that I think that it is unjust and unbusinesslike for a jeweler NOT to inform a costumer that their "white gold" is rhodium plated. The thing is - most jewelry salesman do not exactly know what their "white gold" is made of or in fact what their manufacturer uses in their "white gold". I know many people who have white gold rings in which have never yellowed in years. I have been to numerous jewelry stores and they have all stated that their "white gold" will never show any yellowing in time. Some have never even heard of something like this happening. Someone is misinforming these sales personnel.

I received a $6000 dollar "white gold" engagement ring and never thought I would encounter such problems with such an expensive ring. I had the ring 2 weeks and noticed a yellowing of my ring right after washing dishes. I immediately returned the ring and the salesman said it was the lights in the store. I knew he did not know that he was talking about. I talked to another associate and they said it need to be "re-rhodiumed". Then I felt as if my fiance had been taken advantage of. They sent it off and it looked wonderful and new. Then I got it sized about 2 weeks later and when I went to pick it up, it was as yellow as I have ever seen it. I can't believe the salesman didn't see that before he called me to tell me it was ready to be picked up. I have had the ring for 7 months and it has been re-rhodium plated 5 times. The last time I requested a heavy plating instead of their "flash plating" they do since I have heard that this may last a lot longer. It lasted a bit longer but not much. I am so outraged that I have been through so much problems with this ring.

The store calmed me by ordering a platinum ring that looks identical and charging an additional small price to exchange. It looks great but now I am hearing that platinum will scratch up very quickly. Is platinum all that harder? Am I going to be dissatisfied with platinum now too? How easy is it to polish the ring to it original shine after it scratches? How is a ring marked to ensure it is platinum? PLT ,PT. Is platinum the way to go? Nickel must be removed from the jewelry business for good.

Dina L [last name deleted for privacy by Editor]
- Omaha, Nebraska


++

Platinum is nore precious than gold and I doubt that it will ever be a problem, Dina.

You are right from top to bottom. Some jewelers, whether it's due to duplicity or simple ignorance, are selling consumers $6000 rings that are a major problem quality-control wise, and which also cause the well known and long recognized disease of "nickel itch".

And to make it worse, then they often start in with this 'special sweat' nonsense, trying to make the wearer feel guilty for having some kind of shameful defect in their sweat glands that destroys heirloom jewelry :-)

I usually have little sympathy for trial lawyers and consumers who want to sue at the drop of a hat, but not this time. Eventually a major jewelry manufacturer or distributor is going to make a lawyer rich with a class action suit over rhodium plated gold, and they will richly deserve it. I still pass by jewelry counters full of rhodium plated white gold rings that are not identified as plated. If the underlying white gold was of the highest "whiteness value", it might not be a problem; but the underlying gold is often rather yellowish.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++

I am curious, Ted.... I have a "white gold" engagement and wedding band. I have worn the wedding band for 18 years and it hasn't changed color. It is whiter than yellow gold, but yellower than sterling silver. Does this mean that it probably *isn't* rhodium plated? I have never noticed an "itching" problem, but I am not sensitive to any metals that I know of. I even had a nickel/silver ring once and that caused no problems.

Does white gold get its "white" color from more nickel or chromium? What alloy is high-quality "white gold" supposed to be made of? Do they mix platinum in? My ring was designed locally and sent to a foundry that the jeweler normally used for all of his castings (lost wax process). I have been perfectly happy with it. Was white gold made differently 18 years ago? I suspect that it is nickel that they mixed into the gold, since the jeweler told me it would be harder than yellow gold.

Ronna Erickson
- Amherst, Massachusetts


++

I was totally ignorant about this subject until a couple of years ago, Ronna. I've read a great deal in the meanwhile.

In brief, gold is an element that is always yellow, there is no isotope which is white. White gold jewelry is an alloy made by mixing gold with other metals, most notably nickel or palladium because these have the ability to "bleach" it. The resultant color is whitish, but it can vary and there is a recognized scale of whiteness. These days white gold is usually rhodium plated for the popular dazzlingly bright white look, and what apparently happened was that the "we're going to plate it anyway" mentality let jewelers talk themselves into using white gold of lower whiteness under the rhodium than in the old days when white gold rings were not rhodium plated.

The issues revolve around at least four different problems:

Our FAQ about white gold includes a lot of good responses from jewelers, plating engineers, and others.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+++++++

I have the same situation with my white gold rings. My rings are only 6 months old and the bottom of my rings are turning a little yellowish. I went to the jewelers and I questioned it and they told me that the rings have some nickel in them and maybe I was allergic to nickel. I found out I was allergic to nickel about a year ago when I had a crown put in and I was getting swollen gums and I had to replace my crown.

My question is, could this be the reason my rings are turning yellowish faster than what they should be? Also, is there anything I can take either a vitamin or anything to prevent it? Or I just really need to replace my bands with platinum.

Do you have any suggestions?

Adriana V [last name deleted for privacy by Editor]
- Chicago, Illinois


++

Vitamins will not relieve a nickel allergy, but ingesting medicine to try to bring your body into alignment with your jewelry would be the wrong answer even if it worked :-)

There really should not be nickel in new jewelry anyway as it has been banned in much of the world (not the USA), and a product which is widely recognized as being dangerous should not be sold. It is dangerous because it causes nickel allergy that persists for your lifetime. But here in the USA product design sometimes seems to be driven more by personal injury law rather than proactive innovation.

If the rhodium were thick enough, there would be no yellowing for a longer period and the leaching through of nickel would be somewhat reduced but not eliminated. The problem is not your 'nickel itch', and don't let a jeweler get away with claiming such! Your allergy to nickel is the result of your being assaulted by nickel, and it's quite possible that everyone would acquire this disease if exposed to enough nickel. The problems are:

Good luck.
pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++

I, too, am experiencing discoloration on my white gold ring band. I had my 18k white gold engagement ring resized. The Jeweler who resized it had informed me that it might be rhodium plated. The ring went into the jewelry shop in perfect condition. When I got it back I noticed that there was discoloration on the band. Tiny little white/copper colored dots have appeared all over the band but appear centralized around the area where the resizing was done. Are these dots due to the process used to resize the ring? Could the method used for resizing have damaged the rhodium thus leading to discoloration? According to the jeweler who resized the ring these dots are a manufacturer's defect. Is this true? I have only had the ring for 3 months. From what I have gathered from your site it should be a year before it has to be replated. Why would it tarnish so suddenly? Thank you for your help in this matter.

Regards,

Katherine T [last name deleted for privacy by Editor]
- Montreal, Quebec, Canada


++

You are a customer who is easy to please, Katherine. All you are asking is that your ring survive a year or more between replating. I would be very unhappy if a ring lasted less than 5 years before needing work :-)

But you should not be having to try to figure out exactly what went wrong, and we probably can't do it from this distance. We can guess that the rhodium got burned off or worn off by the tooling or the ring was made bigger and the replacement material not plated--but that's all a guess. The point is that the ring is 3 months old and is now defective due to error on the supplier's fault or the resizer's fault. I would tell the resizer that he broke it and must fix it; he'll probably rhodium plate it.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+++

I'm trying to find some information on this, but all I seem to find is that platinum is supposed to resist most (if not all) kinds of yellowing or tarnishing.

Well ... I received my platinum engagement ring on New Year's Day. A week or so later, I noticed that the base of the prongs, where it connects to the band, has started to yellow. The ring is stamped PLAT (which I read means that it is at least 95% platinum), so I was dismayed that it started to discolor so quickly. The ring was custom-made by my fiance's family jewelers, and when we spoke to them over the phone (they are in Ohio, we're in California), the only explanation they could give was that it could be the solder used to connect the head to the band. They also suggested trying a little Tarn-X [linked by editor to product info at Amazon] but that didn't do anything. I take the ring off when cleaning and washing dishes, but usually leave it on when I normally just wash my hands (with regular soap).

So now, it looks like our only option is to send the ring back and have them fix it (although I'm not quite sure how they're going to do that, without mildly recreating the ring). If anyone has any other suggestions -- or even guesses as to why this happened -- please let me know! I'd rather not part with my new ring! (I know, it's better to get it fixed now, but still, I'm sentimental.)

Help! And thanks ...

Maria V [last name deleted for privacy by Editor]
- Orange, California


+++

I'm having the same problem with my Platinum ring. The solder area between the prong and the band is yellowish. I noticed the discoloration about 3 months after I bought it. Does anyone know why?

Phuoc Luu
- San Francisco, California

Ed. note: The following, from one of this site's supporting advertisers, goes a long way towards explaining the situation with white gold and rhodium plating. You may wish to contact them for further information, advice, and possible services on white gold and rhodium plating issues--


++++

Can rhodium plating disappear on the whole ring when resized? I hope someone can explain the following to me.. I can't seem to find any information online...

I had two rings resized recently and to my amazement and anger, both rings had changed color!

Ring #1 has a white gold shaft but the "flower" design of the ring had a rose-gold rhodium plate finish on it to make it look like petals. When I received the ring, the rose-gold had disappeared and the white gold had shown through. How is this possible if the shank had to be made larger? The person I spoke to said it was due to the heat of the soldering. I can't see how the whole ring changed color.

Ring #2 has a yellow gold shaft but the "flower" design is white rhodium plated. The shank of the ring had to be made smaller. When I received the ring, ALL of the white plating disappeared and the yellow showed through.

Please explain this phenomenon! I never thought that ring resizing would completely take out rhodium plating.

Laura W [last name deleted for privacy by Editor]
consumer - Glen Cove, New York


+++++++

I own a 9K white gold engagement and wedding ring. I have had it Rhodium plated within this month(September 2007) and have noticed a yellowing tinge to the bottom of my rings. I do try not too work too harshly with my rings but I have noticed some fine to medium scratches on the bottom and sides of my rings. If I have them replated, would the rhodium plating damage my rings in the long run? How often could I rhodium plate my rings without wearing off too much gold by the polishing/buffing process? Will the rhodium plating remove fine/medium scratches? Please help me, as I am very distressed and want to ensure that my rings are well cared for.

Inga G [last name deleted for privacy by Editor]
Customer - South Africa


March 11, 2008

I want to say that my husband and I are beside ourselves regarding both my wedding ring & engagement ring. I don't even want to go there is essence of the hardships we had with two different custom Jewelers on Long Island, both highly recommended. Well both rings are white gold, not Rhodium dipped. Both were also appraised after we purchased them and the value is high on both, so we know we got what we paid for. I had to get a V band instead of a regular solid round band for my wedding ring as my engagement ring had two outside stone, so we designed it with the jeweler and it came out very nice. But the first issue is why is the top of the wedding band ( the side that is facing the engagement ring getting a discoloration on it, that are not rubbing, its looking like it may be a chemical reaction to the two pieces of white gold facing one another, its discoloring my ring and my band isn't yellow yet, as its only about 6 months old, but my engagement ring is turning a bit gold. Help, is it safe to rhodium plate over the white gold. As I said it was appraised and is all white gold. Not sure what to do, will the Rhodium finish damage my ring. Will it give it the shine and sparkle it so deserves. also I clean my rings at least once a day is this a safe thing to do with diamonds and white gold. If so what is the safest solution to us for cleaning.
Help-I'm at my wits end right now the rings total 17,000 together.

Kristy W.
Consumer - Smithtown, New York


March 11, 2008

Yes, the rings can be safely rhodium plated and they will be dazzling. Discuss the plating in detail with one of the two jewelers or with Metal Arts Specialties / Artisan Plating.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


June 27, 2008

I have just had my wedding band rhodium plated. It appears to be more like a platinum coloured ring and not the "white" gold colour I was hoping for. The shop assistant told me that the darker colour was a result of the high quality products used. Is this right?

Catherine Peers
buyer - Sydney, Australia


July 2, 2008

Most likely not, Catherine. It's more likely the result of a contaminated rhodium plating solution than a super quality one :-)

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


January 7, 2010

I took my engagement ring into a department store instead of where we got it in order to save a buck and have it resized. I also took another ring given to me to be sized as well. Both of them came back rhodium plated! I want it off of my ring ASAP. They even plated it over my yellow gold part of my two tone ring. I about died. I told them that I was having them sized and specifically told them to NOT plate my rings. The manager acted like they did me a favor in doing so. I told her:

I bought and wanted gold for a reason. It is shiny alone. I love the classic white gold/yellow gold look. If I scratch it, I will pay to get it cleaned and polished by a good jeweler right? What did our grandma's do for crying out loud! It is called good old fashioned maintenance.

I think any jewelry plated with anything should be labeled as FRAUD and jewelers should have to state that it is plated with it. Anything plated with anything cheapens jewelry.

The reasons above are WHY I would rather go to Chicago and get my wedding ring from Tiffany & Co. They don't sell nickel and rhodium rings there. I truly believe you get what you pay for. When we bought the ring it was perfect and NOT rhodium plated. Too bad my finger had to grow a little.

J C Penny's is sending the ring back to be polished supposedly. I told her I wanted the rhodium removed. It looks dull and I hated it when I went to pick my rings up. I cried for a week. Now I am just playing the waiting game. I hope and pray to God they just restore my ring back to the way it was.

Do you think they will and how would they go about removing the rhodium plate?

Teresa Pinkerton
Consumer - Cedar Rapids, Iowa


January 7, 2010

Hi, Teresa, sorry for your troubles. Some people love the look of rhodium plating: no solid metal can ever come anywhere close to the scintillating dazzle of rhodium plating -- so I don't call it fraud nor think it should be outlawed. But I certainly agree that all plated rings should be labeled as such so people can choose intelligently!

The jeweler should certainly not assume it is okay to turn a two color ring into a single color! You are not alone, see letter 53900. Rhodium plating probably cannot be chemically removed, but can be carefully polished off (see letter 10337). Good luck.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


April 9, 2010

Another option I don't hear anyone talking about is palladium . It is in the same family as platinum but far less expensive. Like platinum it is very white (although slightly more gray then platinum ) and will stay white . Also it has no nickel in its alloy which some have an allergic reaction to in white golds . If you don't want to spend the money on a new ring you can ask a jeweler to first palladium plate your jewelry before rhodium plating it. This will make for a thicker plating which will not ware off as quickly . A good plating job should last at least a year , but is something that will have to be repeated . A good jewelry store should offer free maintenance on your jewelry for life , if not you bought the piece from the wrong store, sorry.

Jimi Fortune
- Grass Valley, California


December 10, 2010

As a gift from my mother-in-law I'm receiving her grandmothers engagement ring to use as my own. We are having it sized and cleaned, as it is almost 100 years old. The jeweler told me in order to get the ring as bright as my wedding band, which is brand new, they are going to have to rhodium plate it. is this a bad idea? even though the ring is very dirty it doesn't seem to have any yellowing to it. once the plating starts wearing off will it look more yellow? this ring is far more special than any ring I could have purchased new and do not want to ruin it. is having it plated a bad thing?

Tasha Caruthers
- belle chasse, Louisiana, usa

December 12, 2010

Hi, Tasha. It sounds like your ring is platinum or unplated white gold. The rhodium plating will not "yellow" it, it will make it dazzling white. If the plating wears off in spots, those spots will return to the former color of the ring. But it won't wear off uniformly, so you will need periodic replating; and the plating can be quite tedious to polish off if you change your mind.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search