Letter 14082
Galvanic Corrosion between Nickel Plating
and 17-4 SS
We are designing an instrument that uses nickel-plated
neodymium-iron-boron magnets in contact with 17-4PH stainless steel.
The environment may involve intermittent, temporary exposure to
electrolytes such as saline, and the instruments will be repeatedly
sterilized in autoclaves. We are not concerned about corrosion of the
nickel plating by itself, we are concerned that it could be a problem
where it touches the stainless. Is there a problem with galvanic
corrosion between nickel plating and 17-4PH stainless steel?
Edmund Loftus
- Gainesville, Florida, USA