Polish Motorcycle Rims
Can someone tell me how to polish the inside of my motocycle rims, I have a Suzuki RF900 1994.
THANK YOU
Ron Tucker- Piscataway, New Jersey
+++++++
Ron,
First thing is to get paint remover and strip away the paint. Before doing that though make sure you cover the part that you are not going to remove. After stripping the paint, you should use ultra fine
sandpaper [linked by editor to product info at Rockler] to clean it all up and get out the lines. Finally polish with
Mother's Aluminum Polish [linked by editor to product info at Amazon].
- Piscataway, NJ