Black Dull Nickel Plate  

 

I need to specify Black Dull Nickel Plate as a finish on brass base metal for military use and have been unable to find a supplier or specification/standard for this finish, can you help?

Mr Roger Welland
- Godalming, Surrey, U.K.


 

If you coat a dull nickel deposit with any black layer (like black zinc-nickel or black tin-nickel or even black chromium) it will give you a dull black finish. Maybe you are referring to a satin nickel deposit with a black layer for decorative purposes. The nickel layer is the one who is responsible for the dullness.

 
Sara Michaeli
    chemical process supplier
Israel


 

Attn of Sara M,

Thank you for your time and information regarding Black Dull Nickel Plate, this should enable me to proceed.

Regards,

Roger Welland
- Godalming, Surrey, UK


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search