Wire Rod Defects

 

I am working in a wire rod mill in production department. I am looking some reference material on "Wire rod Defects" such as seams, cracks etc.

Nikhil Nafade
- Hawkesbury, Ontario, Canada


 

Have you checked the trade magazines such as Wire Journal? I am at home so can't give you any other magizines to check. I have an article from a German magazine I believe that explains wire breaks and their causes. I'll look for it tomorrow and see if I kept the reference for it.

Gerald D. Smith
Little Falls Alloys, Inc. - Bloomingdale, New Jersey


 

I am working in a wire rod mill in Quality department. I can help you about your question, but I need some information, If you consider it to be suitable. I wait to be able to help.

Regards,

Alfredo Orta L.
- Saltillo, Coahuila, Mexico


++++++

I saw a coil of wire rods with edges formed along the length of the wire. I would like to know what this defect is. Kindly help.

Jayakumar
Insurance survey - Dubai, United Arab Emirates


+++++++

I have got a very useful book, written with 3 language. You can search the item in like this "wire rod defects Verlag Stahleisen M.B.H. Düsseldorf". You can find this book.

Book name; Walzdrahtfehler, Wire rod defects, Les defaults dans le fil-machine,.
Verlag Stahleisen GmbH, Düsseldorf, 1973
ISBN 3 514 00134 0
ISBN-13: 978 3 514 00134 3

web address:
www.woodheadpublishing.com/en/book.aspx?bookID=190

Hussam BASTUG
isdemir iron and steel co. wire rod mill - Iskenderun, Hatay, Turkey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search