Etching on Iron

 

I need to etch on Pad printing plate (Onhs or wps ) can any body tell me the process and from where to procure these chemicals etc. - please help.

Sunjay Jain
- Mumbai, India


 

You need to coat plate with photo sensitive lacquer. Then expose film of what you want to get on plate. Rinse after exposure with suitable developer. You may need stop off at some place. Once image is created on plate, etch with dilute FeCl3. You must have meshed film. i.e. suitable screen of 133 or 150 mesh will give you image. Ink will retain in mesh. For long life, chrome plate after etching.

Payal Mag
- Charlotte, North Carolina


 

Sunjay:

What Mr.Payal told you is state of the art, but there is an economical alternative, though more difficult and less precise. See my reply to Avner (letter 13531). This might work for you.

Guillermo Marrufo
Monterrey, NL, Mexico

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search