Seeking 6063 cathodes for anodizing tank
Can anyone tell where I can find small quantities of 6063 cathodes for Al anodizing?
Mike Evers- Rockford, Illinois
Mike
6063 T6 isn't a readily available alloy in the T6 form. To get certified material usually you have to have it extruded at a minimum of 1000 lbs. That's a lot of material for most anodizing operations. The good news is we have our special extrusion certified to 6063 T6 in stock at all times. No minimum. We also have it in 1.5" and 2" X 4" as header bars to attach the extrusion to.
|
Drew Nosti, CEF Ladson, South Carolina |