Letter 13025
Seeking source for application of Deltaseal
Coating
My company is a die caster and our customer is requiring a
"Deltaseal" coating on a very small part. They call is out as
follows: Coating: 1X Deltaseal, 0.005 mm - 0.02 mm Thickness, Color:
Silver. The material of the part is ASTM B86, AC41A (ZAMAC 5).
My first question is: Is there a company in Taiwan or China that
applies this coating, if so, who and where? Is this product spayed on
dipped, spun or what? If it is applied in various methods, which is
best for keeping the coating from bubbling?
Note: A 50 hour Salt spray test per ASTM
B-117 [link is to spec at TechStreet] is required, with no
base metal corrosion allowed.
Thank you very much!
Lyle Gallagher
- Gold Canyon, AZ
Ed. note: Delta-Seal® is a trademark of Dörken and
they make be able to help you source this. Alternately,
Met-Fin Supplies represents a large
number of Chinese plating shops, some of whom may offer this
finishing service.
Dear Reader:
Sorry, but this particular Commercial Inquiry / RFQ is outdated.
- Please feel free to:
- Post a Question or Inquiry of your own,
-
- View current RFQs at
- "Seeking Jobshop Services"
- or
- "Seeking Products or Services for Finishing Shops" or
-
- View current technical inquiries on the
- "Hotline - Letters page".
 |