We are manufacturing Surgical Instruments and for stamping
(etching) purpose I need to know how I can prepare etching solution for both Magnet and Non-Magnet Stainless Steel.
Thanks,
M.Zubair
Lloyds&Sons (Pvt)Ltd - Sialkot, Pakistan
Try a Hydrochloric / Hydrofluoric acid mix (30% HCl, 30% HF, 40% water).