What is DIN 50960 plating?

 

I am trying to find information on DIN 50960 plating. What exactly is it (tin/nickel/zinc/etc.)? Is there a website where I can find more info or the full specs?

Thad Rosenberg
- Redwood Falls, MN, USA


 

Thad -

This standard, as well as most others, can be obtained from Global Engineering.

Cynthia L. Meade
- Sylvania, Ohio, USA

. . . or follow the link to DIN 50960-1 [link is to spec at TechStreet]. Techstreet offers finishing.com a small commission which covers our time, so we can save you a step by linking directly to the particular spec in question.

I don't believe that DIN 50960 is a particular type of plating, but a document about how to specify plating.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search