AISI904L = Uranus B6 ?
Is AISI904L and Uranus B6 are equivalent, what about using
AISI904L in phosphoric, sulphuric acids and ammonia atmosphere?
Srinivasn Nagarajan
M/S Ceecons - Chennai, Tamil Nadu, India
Hello Srinivasn!
Well, a simple search on Google turned up a site which cross
references Uranus B6 as 904L. So at least one company thinks they're
equivalent. Then, going to Allegheny Ludlum will give you some
information on 904L. Caveat reader!
|
|
Lee Gearhart
metallurgist
East Aurora, NY
|