Inline Testing of Fluoride 

 

I am looking for a way of inline testing of incoming waste waters for fluoride. My waste treatment operators get slugs of waste from the hydrofluoric etching operation, we are looking for an indicator to tell them they have a problem.

Rick Stinnett
consumer electronics - Marion, Indiana, USA


 

Rather than trying a hardware solution, such as fluoride selective electrodes (an automated system could run big $$$) why not just get the people dumping the concentrates to let you know when they are going to do it?

Bill Vins
microwave & cable assemblies
Mesa (what a place-a), Arizona
 


 

It sounds like you may need a larger equalization tank! If that is not possible, then there are a couple of ways to get the alarm/notice you are looking for. The simplest and cheapest way is to install (fluoride resistant) conductivity sensor in your waste line. Any spikes will also have a much higher conductivity.

There are also two manufacturers of Fluoride analysers that can work over a very large concentration range and are in daily use at many semiconductor companies.

Lyle Kirman
water treatment systems - Cleveland, Ohio


Dear Reader, please --

Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 

 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com