Coating stainless steel

 

We are attempting to use a cyanoacrylate adhesive to bond a stainless steel part to a rubber part. The glue will not adhere to the stainless steel. I would like to know if anyone has a suggestion regarding coating the stainless steel with an aluminum rich coating (ARC) in order to accomplish this.

James Henson
Cooper Tire & Rubber - Bowling Green, Ohio


 

Try using a glue called Sicomet. I used it succesfully to bond stainless steel to rubber.

Sergio Lievano
- Santa Ana, California


 

Our company is trying to do the same thing, bond rubber to a 17-7 stainless steel and we're having mixed results. We're using a chemlok 205 primer with a 250 adhesive. We're cleaning with MEK / methyl ethyl ketone [linked by editor to product info at Amazon].

If you find anything else that works well, please pass it along.

Thanks and good luck.

Elmer Lee
- Ann Arbor, Michigan, USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search