I would like to know about the micro gold plating. Kindly suggest me some good magazine and journals as well as books available on this topic. I am keen to learn about technical aspect of micro gold plating.
Manoj Kumar- Patna, Bihar, India
What do you mean by micro gold plating?
Michael BrewingtonFin-Tec, Inc. - Salisbury, Maryland, USA
Hi,Manoj Kumar,
I believe that "Micro Plating" is just a trade name like Coca Cola or Windows.

Dipen Pattni
jeweler/goldsmith - Dar-Es-Salaam, Tanzania
Do you mean flash gold /Immersion gold? The plated film thickness will be in the order of 0.05 microns.
V.RAMANAND KINI- Bangalore, India