What is Scotch finish?

N Gopal
extrusions - Dubai, U.A.E


 

Dear Mr. Gopal:

I would say that it means to abrade the surface with a fiber manufactured by 3M called Scotch-Brite.

Guillermo Marrufo
Monterrey, NL, Mexico
 

The fellow from Mexico is right. The proper name for this material and these synthetic fiber wheels and belts are referred to as non-woven. Scotch-brite is 3M trade name.

AF Kenton
Huntingdon Valley, Pennsylvania

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search