Letter 11089

Stripping Nickel-P Coating 

 

Dear Sir:

I am a research student for Nickel-P electroless plating. I want to strip the Nickel-P coating without damage the copper or Aluminum substrate. Is there any solution suitable for that? I have tried to strip the EN Nickel coating by 1:1 nitric acid, unfortunately, It seems that nitric acid is too strong for copper than the EN nickel. Finally, I find the Cu substrate, which is about 0.1-0.2 mm, is eroded by nitric acid through cross-side.

Xu Xiaoda
NTU - Singapore

Editor's note: Metalx offers such a stripper.


Dear Reader, please --
Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com