Does anyone know a process for chemically or molecularly bonding a
copper plate .0020" thick to a steel plate .0008" thick? It must be
able to withstand heating to 400 degrees F on a regular basis.
Michael Wilks
- Newton, Kansas, USA
Does it absolutely have to be steel? Electroplating the copper
with nickel would seem to be a very straightforward answer if nickel
can do the job.
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|