finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 11067

Glass coatings colors

 

Dear Sir,

I am an artist. I am working glass and I want to make some colors at the surface. I want to do these coatings by spray below 650 deg. C. Have you some informations to produce red coatings, blue coatings, black coatings and white coatings? Thank you very much.

Sophie Labatut
- Paris, FRANCE


 

Why don't you try simply using spray paint and some sort of stencil? What kind of requirements do you have? Are you looking for coloring you can see through similar to stained glass?

Tim Neveau
Rochester Hills, Michigan

 

Why don't you experiment with colored vitreous enamels, rather than attempting a top color. Go to the www.thompsonenamel.com website for more info.

George Brackett III
- Utica, New York


 

Please check www.glasskote.com website. It may be of interest to you. The coating involved here is now being used widely around the world. It does not require any baking at all. Thank you Steven

Steven Vas
Euroglaze (aust) pty ltd - Australia


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search