Electropolishing Tungsten

 

I am interested in finding a process that would be suitable for electropolishing Tungsten, including any pretreatment processes that may be required.

David Binks
- Bordon, Hampshire, UK


 

There are different methods of electropolishing Tungsten, the low-voltage method is pretty environmentally clean. It depends on the type of alloy you want to polish.


Anna Berkovich
Russamer Lab

Pittsburgh, Pennsylvania


May 12, 2008

I'm also looking to electropolish tungsten, specifically tungsten-rhenium.
Information on the electrolyte and its concentration, current density etc would be very helpful

Maryanne Muriuki
- Somerville, New Jersey

^-- I want to contact this person and my company is a supporting advertiser of finishing.com

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search