HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 11020
Article 669-Electroplating
Dear Sir:
Can anyone advise me in Article 669-Electroplating in the National Electrical Code what is the coverage of this article refer to.
Regards,
Ron Henka- Singapore
It refers to the physical plant that uses and distributes current to the electroplating and anodizing lines, for safe installation. You can order a copy of the NEC for your information.
|