Surface Tension
Please let me know the surface tension of ethylene glycol (pure) and its polar and dispersive components.
Best regards,
Sourav KumarIndian Institute of Technology, Kharagpur - Kharagpur, West Bengal, India
November 16, 2008
The surface tension of ethylene glycol at 25C (298.15K) is 48.4 dynes/cm. I do not know its polar and dispersive components a this time.