Is it Galvanized or Galvannealed?

 

What is a simple way to tell the difference between metal that is galvanized or galvaneeled?

Paul L [last name deleted for privacy by Editor]
- Manchester, Iowa


 

GALVANNEAL Carbon steel sheet with a fully alloyed iron-zinc coating on both sides. I don't know if you would consider it simple, but it may have a different galvanic potential compared to some electrode.

tom portrait
Tom Pullizzi
Falls Township, Pennsylvania


 

Galvanizing, where 100% Zn on the top surface of the steel,where as in Galvannealed,90-93% Zn with 10-7% Fe on the top surface. The simple way to distinguish is that Galvannealed material will look like matte finish, where as Galvanized material will look like bright finish.

Tapan K Rout
- Jamshedpur, India

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search