Layman Needs Plating Guidance

--

I'm not in finishing industry. However, I need info on PTFE, Titanium Nitride, and Diamond Black coatings for IC manufacturing equipment wear parts.

I am also looking for local supplier in Phoenix, AZ area (or somewhere in Southwest US at least) to work with.

Tony S [last name deleted for privacy by Editor]
Motorola


--

PTFE can be applied by spraying, dipping in fluidized bed, etc; it can also be applied by co-deposition during electroless nickel plating, and that represents a very good wear surface.

Titanium nitride is actually a vacuum process, not plating, and SVC (www.svc.org) can probably help you.

Regarding diamond black, please see letter 582.

Of course the most traditional wear surface for most equipment parts is probably hard chrome plating. Good luck.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey

ASM vol5
ASM Metals Handbook vol. 5

Surface Engineering

Mallory book
Electroless Plating - Fundamentals & Applications,

Mallory & Hajdu

guffie book
Hard Chromium Plating

Robert K. Guffie


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search