Brake Caliper and Piston Plating
--
Does anyone have knowledge on the type of plating generally used on automotive caliper pistons. Some have told me its a chrome finish but others have said its Cad.
Thank you in advance!
Tom--
I thought it was Electroless Nickel.
David M. Weaver
- Toccoa, Georgia
Ed. note: With sadness we must advise that David lost his life to a car accident on Aug. 15, 2003.
-
Depends on the make and era of your car. I know that GM power brake "boosters" were "gold cadmium dichromate". This is also used on the brake backing plates of some GM cars. I am looking for a supplier to do this as well. Many car brackets are also done in the g-c-d process. Car judges will accept black or natural finish metal for the calipers on 60's GM cars