Looking for books on Electropolishing of metals

---

We are a company working with metals, and are now looking to expand our expertise into high level Electropolishing of metals.

I am looking for more information and books (new books if available) on techniques, theories and procedures in that field.

Thank you,

Ehud Goren


---

Mr. Goren:

Please see our listing under "Software, Training, and Education" on this web site. There you will find a summary of topics discussed in monthly seminars held in Charlotte, NC. Seminar materials include a comprehensive technical manual covering most of the topics you mention.

For the schedule of future seminars and a detailed program, please refer to our web site.

Ed Bayha
Metal Coating Process Corporation

Charlotte, North Carolina, USA


.

Dear Sirs, I need books on stainless steel electropolishing,methods and chemical compositions,Please refer me the best book name or the company for such techniques and methods. Thanxs.

Shakel Ahmed
- sialkot, Pakistan

----
Ed. note 10/22/04:
We don't think there is an electropolishing book in print anymore, but you can get a used copy of Tegart's "The Electrolytic And Chemical Polishing of Metals"
 
Alternately, the Electroplating Engineering Handbook has a great chapter on electropolishing.


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com