Coating ID of capillary tubes with polysiloxane / silicone

--

We are attempting to coat the inside of brass and stainless steel capillary tubes (approximately 250 Microns I.D.) with a polysiloxane (silicone) coating. We are having difficulty getting a uniform coating and am looking for a procedure to produce same without defects. We currently do not use and pretreatment or passivation of the metals (brass and stainless) and have been attempting to coat by drawing a dilute 3% solids polysiloxane coating through the tubes under vacuum and exhausting the residual solvents to complete the coating/curing process.

Can you recommend a process for cleaning and passivating the surfaces of the brass and stainless that would give satisfactory results with subsequent coating. Capillary tubes are for gas chromatography column use.

Any assistance would be appreciated.

Dave Reim
- Columbus, Ohio


.

Not all polysilaxanes are currently being marketed. The ones that are not must typically be licensed from a patent holder. On the web you can find abstracts of many of these patents and can contact the patent holder after getting the phone number of the patent holder from the Patent & Trademark Office. Currently I am looking at one particular polysilaxane for our project that has a clear optical finish (our requirement) but requires no fillers, thus the chemical has a higher modulus, goes on differently, and is even harder than others once cured. I am not a chemist, but it could be that fillers are interfering with adhesion in your application.

Christina Duncan
- Dallas, Texas


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search