Treatment of spent silver baths

--

i wonder if anybody could inform me on practical experiences with costeffective treatment of spent cyanide containing silver baths with max recycling (electrolytic with subsequent ion exchange)

regards and thanks, gert

gert holm kristensen
Malaysia


--

Is it necessary to treat at your facility? The best bet is to send it to a reliable recycler who specializes in this processing.

The use of electrolytic recovery on-site makes sense if you will be following it with chemical destruction (ozone or hypochlorite) then precipitation. No sense making a silver chloride or silver oxide laden sludge when you can cut the weight and volume by over 90% by getting the silver out as metal via electrolysis.

Chemical means are also available for precipitating the silver as silver metal before final cyanide treatment. Unfortunately they will also increase sludge volume since they usually involve zinc or aluminum as reducing agents.

Never run a concentrated bath through ion exchange. It will either break through immediatly, or at best, will exhaust the resin much sooner than necessary. Then you have to regenerate the resin, and if doing it on site, you are back where you started with a concentrated cyanide solution.

Bill Vins
microwave & cable assemblies
Mesa (what a place-a), Arizona



ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search